Thick sheet blister: solution to the difficult problem of blister

Time: 2020-11-05

Summary:Yangzhou tubo blister factory is a professional engaged in blister products manufacturing enterprises, providing taizhou thick sheet blister, thick sheet blister shell, medical chassis processing, medical equipment chassis, thick sheet blister processing, yangzhou thick sheet blister, yangzhou paint processing technology services, the production of various colors of ABS, PETG, PVC, PC, PP, PE, HDPE, PET, ABS/PMMA, ABS/PC, etc. and a variety of modified plastic light plates, leather grain plates, transparent plates are mainly vacuum blister molded, with a thickness range of 0.2-10mm. All product molds are designed and developed by themselves.

1. Thick blister hanging wire: when thick blister is formed, a wire frame bulges will appear on the edge of the blister product due to the aspect ratio of the die shell, its viewing angle, the structure of the release, etc. In case of serious damage to the appearance, it will generally be solved as a residual product.

2. Thick sheet blister tone: the difference in tone generally appears on the seasoning of the plastic sheet manufacturer. It is very likely that different background color differences will appear on different batches of plastic sheets. However, this kind of situation is not easy to cause great harm and cannot be distinguished in individual packaging. Therefore, this kind of situation focuses on communication with the plastic sheet manufacturer.

厚片吸塑.jpg

3. Hole breaking of thick sheet blister: In the whole process of thick sheet blister forming, hole breaking will occur when the raw material is thin and uneven and the temperature control is unstable. Absorbing products with broken holes are generally regarded as poor products and are not delivered as genuine products.

4. Scratches on thick sheet blister: Scratches and scratches on the surface of thick sheet blister products are very easy to occur. In the processing and packaging process, if the handling is wrong, the surface of blister products will be scratched and marked, which will seriously become a poor product.

5. Blister deformation of thick sheets: The key reason for the deformation of thick sheets of blister products is the occurrence of temperature adjustment, bubble of raw materials, residue and other conditions, which will cause the deformation of blister, fail to absorb in time, fail to meet the regulations of blister forming, and make the packaged objects unable to be put in and become residual products for scrap.

6. Thick blister wave pattern: The key appears in the processing process of plastic plates. The surface wave pattern of PVC plastic plates is more common and can be accepted under general conditions. Large wave pattern will give high-standard packaging waste and become poor goods. Therefore, it can only be improved according to the plastic plate manufacturer.

7. Thick blister bubble: Generally, gas permeates into plastic during the processing of raw materials, resulting in bubble conditions. Under such conditions, bubble stool will harm the appearance, so this kind of bubble will become residual products.

8. Thick Blister TPE: Because during the processing of blister sheet, chemical substances such as residue in raw materials and floating dust in the air accidentally enter the production and manufacture of plastic plates, the produced plastic plates will cause deficiencies and become inferior products.

Key words: Nanjing thick sheet blister, thick sheet blister manufacturers, thick sheet blister processing, thick sheet blister shell